AGESIN® Polyether modified silicon leveling agent
Product Number: AgeSin® LA-D5410
Completely replaced– TEGO Glide 410, DOW CORNING 205SL(50%),DOW CORNING 402LS
Composition | Polyether modified polydimethyl siloxane |
Appearance | slight yellowish clear liquid(paste at low temperature) |
Solvent | PMA |
Density | 0.96-1.00g/ml(25±1)℃ |
Viscosity | ≥U(Bubble viscometer)(25±0.2)℃ |
Content | 92±3%(105℃ 3h) |
Flash point | >70℃ |
This data sheet is intended to give typical results, not standard.Subject to COA.
● Water-based, Solvent-based, UV Cure
● Provide a stronger reduction of the surface tension.
● Reduce the friction coefficient. Increase slip and improve scratch resistance.
● Good recoating and minimal influence on adhesion of coating films.
● Excellent anti-cratering ability, commonly used to replace oil-resistant agent, do not affect the environment and recoatability.
● Hazy and viscous may occure at low temperatures. It would become clear and flow after heated. This will not influence the quality.
Diluted before addition, added in any stage including post-adding.
Suggest addition
Addition to total formulation 0.05-0.5%
Storage stability
Keep intact 24 months in original package.Products beyond the storage period may continue to be used after inspection. The container must be closed immediately after use.
Transparency in varnish : 1
Defoaming : 2
Dynamic surface tension : 5
Static surface tension : 5
Slip : 5
Prevent orange peel : 1
0=unavailable 5=very effective
● 25KG / 180KG
Being kept in dry, clean warehouse with well ventilation.
Avoid exposing to light and heating.
Protecting the product from leakage, rain and insolation during transportation.
We offer a variety of options to help you find the right product for your application
Provide formulation optimization support for water-based/solvent-based systems
Full coverage of REACH, FDA, and GB standards
99.8% on-time delivery rate, 10,000-ton production capacity guarantee